HASTELLOY? X /GH3536(UNS N06002/W-Nr 2.4665 )
HASTELLOY® X /GH3536(UNS N06002/W-Nr 2.4665 )特性:
合金在1200℃的高溫下,仍具有極高的強(qiáng)度和耐氧化性,加上出色的成型及焊接性能,和出色的耐應(yīng)力腐蝕開裂性能,被廣泛用于燃?xì)廨啓C(jī),工業(yè)爐,熱處理設(shè)備和核工程的過程組件,如燃?xì)鉁u輪的燃燒缸、補(bǔ)燃器錐管、過渡管、噴射桿,以及化工行業(yè)的蒸餾,馬弗爐,催化劑支撐格柵,爐膛擋板,熱解操作的管材和閃蒸干燥器部件等。
HASTELLOY® X /GH3536(UNS N06002/W-Nr 2.4665 )牌號(hào)標(biāo)準(zhǔn)名稱:
中國(guó) |
GB/T 14992-2005 |
GH3536(GH536) |
美國(guó) |
ASTM B572-2011 |
UNS N06002 |
HAYNES |
HASTELLOY® X alloy |
|
日本 |
JIS H 4551-2000 |
NW6002 NiCr21Fe18Mo9 |
NIPPON YAKIN |
NAS HX |
|
德國(guó) |
DIN 17744-2002 |
2.4665 NiCr22Fe18Mo |
VDM Metals |
Nicrofer®4722 Co alloy X |
牌號(hào) |
GH3536 |
N06002 |
NW6002 |
2.4665 |
C |
0.05~0.15 |
0.05~0.15 |
0.05~0.15 |
0.05~0.15 |
Si |
≤1.00 |
≤1.00 |
≤1.00 |
≤1.00 |
Mn |
≤1.00 |
≤1.00 |
≤1.00 |
≤1.00 |
P |
≤0.025 |
≤0.040 |
≤0.040 |
≤0.020 |
S |
≤0.015 |
≤0.030 |
≤0.015 |
|
Ni |
余量 |
Remainder |
殘部 |
Other |
Cr |
20.5~23.0 |
20.5~23.0 |
20.5~23.0 |
20.5~23.0 |
Mo |
8.0~10.0 |
8.0~10.0 |
8.0~10.0 |
8.0~10.0 |
Fe |
17.0~20.0 |
17.0~20.0 |
17.0~20.0 |
17.0~20.0 |
Co |
0.5~2.5 |
0.5~2.5 |
0.5~2.5 |
0.5~2.5 |
W |
0.2~1.0 |
0.2~1.0 |
0.2~1.0 |
0.2~1.0 |
Al |
≤0.50 |
— |
— |
≤0.50 |
Ti |
≤0.15 |
— |
— |
— |
Cu |
≤0.50 |
— |
— |
≤0.50 |
B |
≤0.01 |
— |
≤0.01 |
≤0.01 |
牌號(hào) |
GH3536 |
N06002 |
NW6002 |
2.4665 |
C |
0.05~0.15 |
0.05~0.15 |
0.05~0.15 |
0.05~0.15 |
Si |
≤1.00 |
≤1.00 |
≤1.00 |
≤1.00 |
Mn |
≤1.00 |
≤1.00 |
≤1.00 |
≤1.00 |
P |
≤0.025 |
≤0.040 |
≤0.040 |
≤0.020 |
S |
≤0.015 |
≤0.030 |
≤0.015 |
|
Ni |
余量 |
Remainder |
殘部 |
Other |
Cr |
20.5~23.0 |
20.5~23.0 |
20.5~23.0 |
20.5~23.0 |
Mo |
8.0~10.0 |
8.0~10.0 |
8.0~10.0 |
8.0~10.0 |
Fe |
17.0~20.0 |
17.0~20.0 |
17.0~20.0 |
17.0~20.0 |
Co |
0.5~2.5 |
0.5~2.5 |
0.5~2.5 |
0.5~2.5 |
W |
0.2~1.0 |
0.2~1.0 |
0.2~1.0 |
0.2~1.0 |
Al |
≤0.50 |
— |
— |
≤0.50 |
Ti |
≤0.15 |
— |
— |
— |
Cu |
≤0.50 |
— |
— |
≤0.50 |
B |
≤0.01 |
— |
≤0.01 |
≤0.01 |
牌號(hào) |
GH3536 |
N06002 |
NW6002 |
2.4665 |
C |
0.05~0.15 |
0.05~0.15 |
0.05~0.15 |
0.05~0.15 |
Si |
≤1.00 |
≤1.00 |
≤1.00 |
≤1.00 |
Mn |
≤1.00 |
≤1.00 |
≤1.00 |
≤1.00 |
P |
≤0.025 |
≤0.040 |
≤0.040 |
≤0.020 |
S |
≤0.015 |
≤0.030 |
≤0.015 |
|
Ni |
余量 |
Remainder |
殘部 |
Other |
Cr |
20.5~23.0 |
20.5~23.0 |
20.5~23.0 |
20.5~23.0 |
Mo |
8.0~10.0 |
8.0~10.0 |
8.0~10.0 |
8.0~10.0 |
Fe |
17.0~20.0 |
17.0~20.0 |
17.0~20.0 |
17.0~20.0 |
Co |
0.5~2.5 |
0.5~2.5 |
0.5~2.5 |
0.5~2.5 |
W |
0.2~1.0 |
0.2~1.0 |
0.2~1.0 |
0.2~1.0 |
Al |
≤0.50 |
— |
— |
≤0.50 |
Ti |
≤0.15 |
— |
— |
— |
Cu |
≤0.50 |
— |
— |
≤0.50 |
B |
≤0.01 |
— |
≤0.01 |
≤0.01 |
HASTELLOY® X /GH3536(UNS N06002/W-Nr 2.4665 )應(yīng)用:
是主要用鉻和鉬固溶強(qiáng)化的一種鐵量較高的鎳基高溫合金,密度為8.3g/cm3。
> SUS314的卓越應(yīng)用與獨(dú)特魅 ?? ? 2024-09-23
> 309si2/SUS309Si2 ?? ? 2024-09-23
> SUS347集耐蝕、耐熱、焊接 ?? ? 2024-09-23
> SUH330耐滲碳、耐熱鋼 ?? ? 2024-09-23
> SUS321:高溫與氫腐蝕的守 ?? ? 2024-09-20
> SUS310S耐熱鋼璀璨亮相 ?? ? 2024-09-20
> SUH310傲立于1035度高溫之 ?? ? 2024-09-20
上一條:NS3304(NS334)N10276,1.3981,NW0276,C-276 下一條:1.4529(N08926)/926合金 返回列表